Blow-out failure: failure is characterised through the lateral spalling of concrete within the proximity of the anchor's head. This sort of failure occurs for anchors (prevalently Solid-in-spot) installed in the vicinity of the sting from the concrete element.Steel failure: the weak Section of the relationship is represented through the rod. The fa